Welders explained: MIG, ARC and TIG, amps and duty cycle
Checked 19 November 2026
What gasless MIG, ARC and lift TIG mean, how to read a welder’s amp range and duty cycle, why the plug matters — using SIP’s own figures — and what HSE says about shock, fire and fume.
A welder’s spec sheet packs a lot into a few lines: the processes it can do, a current range in amps, a duty cycle, the thickness of steel it suits and the supply it needs. This guide explains each one using SIP’s published figures for the four welders on this site, then sets out what HSE says about the hazards that come with any welder.
Three processes: MIG, ARC and TIG
- MIG. The machine feeds wire from a reel through a torch with a trigger. The SIP WELDMATE 100A is gasless MIG only: it uses 0.8–0.9 mm flux-cored wire on a 0.7 kg reel, so no gas bottle is needed. The WELDMATE 160A also comes set up for gasless MIG, and SIP includes a gas hose with clamps; it takes 0.7 kg or 5 kg reels.
- ARC (MMA, or “stick”). You hold a coated electrode in a holder. The WELDMATE PRO 140A takes electrodes from 1.6 to 3.2 mm and sets the current to suit the electrode you select.
- TIG. All of SIP’s TIG-capable machines here use lift TIG, and on the 160A and PRO 140A the TIG torch is sold separately (SIP suggests its item 08206A). Budget for it if TIG is the reason you are buying.
Current range and steel thickness
More amps means thicker metal. SIP gives:
- WELDMATE 100A: 20–100 A, mild steel 0.8–3 mm.
- WELDMATE 160A: MIG 20–160 A, ARC/TIG 20–140 A, mild steel 0.8–5.5 mm.
- WELDMATE PRO 140A: 10–140 A, mild steel 1.6–7 mm.
- WELDMATE 180A cordless battery welder: ARC 10–180 A, lift TIG 10–150 A.
Match the range to the thickest work you expect to do, not just the thinnest.
Duty cycle: how long it can weld
Duty cycle is the figure that most often surprises new owners. Miller, the welding equipment maker, explains it as a percentage of a 10-minute period: a machine rated at 30% at a given current can weld for about three minutes in ten at that current, then needs about seven minutes to cool. Thermal overload protection shuts the machine down if it overheats. Higher currents mean a shorter duty cycle.
SIP’s figures:
- WELDMATE 100A: 100 A at 15% (at 40 °C).
- WELDMATE 160A: 160 A at 15% MIG and 140 A at 15% ARC/TIG (at 40 °C).
- WELDMATE PRO 140A: 140 A at 30% (at 20 °C).
- WELDMATE 180A battery: 180 A at 10%, 130 A at 20% and 60 A at 100%.
The battery welder’s three figures show the pattern: turn the current down and the machine can work for longer. Note the temperatures too. SIP rates the PRO 140A at 20 °C and the MIG machines at 40 °C, so the percentages aren’t directly comparable — just as noise figures measured at different distances aren’t.
The plug and the power supply
- The 100A and PRO 140A are listed for a 230 V 13 A supply — an ordinary socket.
- The 160A is listed for a 230 V 16 A supply. Check what your workshop has before you buy, and ask an electrician if you are unsure.
- The 180A has a built-in 740 Wh lithium-ion battery that SIP says charges in 1.5 hours. SIP’s estimate per full charge is about 20 rods of 2.5 mm at 85 A, 14 of 3.2 mm at 115 A or 6 of 4 mm at 160 A. SIP advises keeping the battery above 50% charge when not in use and doing a discharge/recharge cycle every three months.
Running a welder from a generator needs care: Honda describes its i-AVR generators, with their stable voltage and frequency, as well suited to welders. See how to size a generator and check the welder’s manual.
What’s in the box
SIP supplies a face shield with the 100A and 160A MIG machines. A hand-held shield is a start, but an auto-darkening helmet with the right filter leaves both hands free — see eye, face and breathing protection for the EN 169 filter standard. The PRO 140A comes with electrode and earth leads and a hammer/brush; the battery welder with an electrode lead, earth lead and carry strap.
Electric shock
HSE explains that arc welding needs a live circuit, so hand-held ARC welding carries a risk of shock and electrical burns; MIG and TIG are lower risk because the current is switched by a trigger or foot switch. HSE’s precautions include:
- check welding and return leads, plugs, clamps and torch or electrode holders for damaged insulation before use;
- clamp the return (earth) lead close to the weld, on clean metal;
- in damp conditions or working on the metal itself, use a dry insulating mat or platform and clean, dry gloves and overalls — remembering that PPE doesn’t prevent shock;
- for ARC welding, prefer machines with an open-circuit voltage limiting device. SIP lists a VRD (voltage reduction device) on the PRO 140A, and a VRD mode on the 180A battery welder.
Fire
HSE warns that heat, sparks and molten slag can travel a long way. Clear wood, fabric, cardboard and other flammable material before you start. Where that isn’t possible, HSE says keep a fire watch during the work and for at least 30 minutes afterwards (up to 60 minutes where a fire could be slow to show). Never weld or cut a drum or tank that has held anything flammable unless it has been emptied and cleaned — HSE has separate guidance on that.
Fume, UV and noise
HSE treats welding fume as a serious health risk. Since its 2019 safety alert, HSE’s position is that all welding fume, including fume from mild steel, can cause lung cancer; that general ventilation doesn’t achieve enough control indoors, where extraction is needed; that outdoor welding needs suitable controls such as respiratory protection; and that no welding should be done without suitable controls, however short the job. HSE also lists UV damage to eyes (“arc eye”) and skin, and noise from arc welding.
Quick checklist
- Choose the process: gasless MIG for simplicity, ARC for thicker steel, TIG if you will buy the torch.
- Check the current range and maximum thickness against your work.
- Read the duty cycle and the temperature it was measured at.
- Check the plug: 13 A or 16 A.
- Budget for a helmet, gloves, fume control and a clear, non-flammable work area.
Search Amazon for 0.8 mm flux-cored MIG wire — check the reel size and wire diameter against your welder.
As an Amazon Associate we earn from qualifying purchases.
General information only. Always read and follow the maker’s manual and safety instructions, wear the protection it tells you to, and keep children and pets away from machinery. This guide summarises official and makers’ guidance; it isn’t legal or professional advice.
Sources
- SIP: WELDMATE 100A MIG welder (05729) (checked 19 November 2026)
- SIP: WELDMATE 160A MIG/ARC/TIG welder (05733) (checked 19 November 2026)
- SIP: WELDMATE PRO 140A ARC/TIG inverter welder (05690) (checked 19 November 2026)
- SIP: WELDMATE 180A ARC/TIG cordless battery welder (05712) (checked 19 November 2026)
- Miller Electric: Duty cycle — what it is and why it’s important (checked 19 November 2026)
- HSE: Safety risks and welding (electrical, fire) (checked 19 November 2026)
- HSE: Health risks from welding (updated 9 January 2026) (checked 19 November 2026)
- HSE: Safety alert on mild steel welding fume and cancer (February 2019) (checked 19 November 2026)
- Honda UK: generator power outputs explained (checked 19 November 2026)
Checked 19 November 2026.